A YASKAWA AR1440 weld fault involving wire stick-out or torch contact should be reconstructed from the torch, feeder and robot path together. A contact mark may result from a changed TCP, a fixture shift, wire-feed behavior or cable resistance. Re-teaching a point before recording the first event can hide the reason for the collision.

Yaskawa lists AR1440 as a six-axis arc-welding robot with a thru-arm cable path and YRC1000 controller context. Those product features do not define the installed torch, feeder, wire, welding procedure or fixture. Use the cell integration drawing and welding documents for those boundaries.

Record the first wire or torch event

Save the joint, job, robot pose, approach direction, wire identity and first message. Note whether the issue appears before arc start, during travel, during wire retract or after a restart. Record the contact location and the last known good torch condition. A later wire-burnback or program stop may be a consequence rather than the source event.

  • Torch and contact-tip assembly identity.
  • Feeder, liner, drive-roll and wire condition.
  • TCP version, tool orientation and path revision.
  • Fixture, workpiece and cable-route changes.

Inspect torch geometry and TCP before reteaching

Under the required cell isolation, compare the torch neck, contact tip, nozzle, mounting adapter and torch angle with the approved assembly. A bent neck or a changed tip extension can move the effective TCP without a robot alarm. Measure or verify the tool using the applicable procedure; do not make a new program offset merely to fit a visibly damaged torch.

Compare the physical tip position with a known fixture feature under the permitted method. Keep tool orientation and sign conventions in the record. A single visual gap cannot distinguish a TCP shift from a fixture shift, and a point that looks correct in one orientation may be wrong at another.

Separate wire-feed behavior from path clearance

Inspect spool path, liner, feed rolls, contact tip and torch cable according to the installed welding procedure. A restricted liner or worn roll can change wire delivery and apparent stick-out. A clear robot path does not prove the wire is feeding correctly, while a feed problem does not explain every collision. Keep the two observations separate.

Check the route at the affected wrist orientation and approach direction. A tight loop or displaced restraint can pull the torch only during a particular move. Do not use a static continuity result to close a dynamic routing complaint; record the route, restraints and dynamic observation separately.

AR1440 torch-fault patterns
PatternCompare nextNot established
Contact after torch changeTCP and mountingRobot calibration fault
Stick-out changes during feedLiner, rolls and wirePath is wrong
Collision follows one approachCable route and clearanceTorch is bent
Same TCP; fixture movedFixture reference and pathDrive fault

Keep weld procedure and robot path evidence separate

Record the approved wire, gas, torch setup and procedure version, but do not infer numerical settings from the AR1440 model page. A weld-quality issue may require process review even when the path is correct. Conversely, an accurate bead does not prove that every clearance and cable condition is safe across the full job.

If the workpiece or fixture changed, compare the new reference with the approved drawing and part presentation. A fixture shift can create a TCP-like error at the torch while the robot data remains unchanged. Record the physical finding before changing coordinates, and keep the old and new fixture references in the report.

Check the wire exit and contact-tip condition after a short, controlled feed observation permitted by the welding procedure. A bent wire path can make the apparent TCP change at the arc even when the torch mount is stable. Keep this observation separate from a full weld-quality test and document the consumable condition before replacing several items together.

For a collision near a fixture, compare the programmed clearance with the actual wire and torch envelope, not only the robot flange path. The wire can extend beyond the nozzle and the feeder or hose can occupy another envelope. Record which envelope was checked and which remains unverified.

Where the AR1440 thru-arm route is involved, identify the cable entry and exit points used by the installed torch package. Product-level routing context does not prove the customer assembly is correct. Compare the actual restraint and bend condition at the event pose, then keep the route finding separate from TCP and consumable findings.

Keep the original torch and wire records until the representative joint has been inspected. Discarding the consumable before documenting it removes useful evidence about the first stick-out change. The report should say whether the repair addressed the torch, feed system, route, fixture or program, and not combine all five into one unsupported cause.

Repair the confirmed boundary and verify the bead

A damaged torch or cable needs its matched assembly and routing repair. A feed issue needs the feeder or consumable service route. A TCP or fixture issue needs a controlled reference correction. Only independent robot motion evidence should lead to an arm or drive diagnosis. Do not call every torch collision a robot repair.

After the agreed work, verify approach, torch clearance, wire response, arc start and representative joints under the approved procedure. Record the repeated cycle count, inspection result and any open process item. A dry path test cannot validate wire stick-out or weld quality, while one visually good bead cannot close a repeated clearance fault.

Welding robot inspection and repair

Contact Suntech with the AR1440 welding record

Manufacturer model reference

Yaskawa AR1440 model and welding information

General checks for welding sequence interruptions